Insufficient impact strength
Release Date:
2023-11-07
-
Possible causes:
(1) Improper resin selection: Insufficient flexibility or low molecular weight of the resin itself results in high brittleness after film formation.
(2) Improper reactivity or dosage of the curing agent: When the reactivity of the curing agent is mismatched with that of the resin, or when the dosage does not achieve the optimal stoichiometric ratio, the crosslink density may become excessively high (resulting in brittleness) or insufficiently high (leading to weak cohesion), thereby reducing the coating’s impact resistance.
(3) Poor system compatibility: Inadequate compatibility between the resin and the curing agent leads to microphase separation within the coating, creating stress concentration points.
(4) Curing temperature conditions not met
Proposed solution:
(1) Adjust the process: reduce the curing temperature by 10–15°C or shorten the baking time by 5–10 minutes;
(2) Formulation adjustment: Add Huanyu HY216/217 curing accelerator.
Previous page:
2023-11-07
Silver powder is unevenly dispersed.
2026-03-20
2026-03-20
2026-03-20
2026-03-20
2026-03-20
Contact Us
Address: Floor 1, No. 373-1, Xiaoyanjialou, Hongta Village, Yongzheng Subdistrict, Jinzhou District, Dalian City, Liaoning Province
Contact number:+86 198 2433 9728
Fax: 0411-87818331
Email: huanyu_additive@163.com
Copyright © 2026 Dalian Aidesi New Materials Co., Ltd. All rights reserved.
图片alt标题设置: huanyu
CSS / JS 文件放置地