Shrinkage porosity
Release Date:
2026-03-20
-
Possible causes:
(1) Contaminated
(2) Insufficient addition of leveling agent
(3) Poor dispersion
(4) External Contamination
(5) Raw Material Quality
(6) Process control or environmental factors
Proposed solution:
(1) If the leveling agent is insufficient, it must be replenished;
(2) For craters caused by contamination, the HuanYu HY518 anti-interference agent can be added to the formulation to eliminate surface tension differences at contaminated spots and enhance the coating’s resistance to contamination. Scope of application: mild contamination or preventive addition.
Previous page:
Next page:
2023-11-07
Silver powder is unevenly dispersed.
2026-03-20
2026-03-20
2026-03-20
2026-03-20
2026-03-20
Contact Us
Address: Floor 1, No. 373-1, Xiaoyanjialou, Hongta Village, Yongzheng Subdistrict, Jinzhou District, Dalian City, Liaoning Province
Contact number:+86 198 2433 9728
Fax: 0411-87818331
Email: huanyu_additive@163.com
Copyright © 2026 Dalian Aidesi New Materials Co., Ltd. All rights reserved.
图片alt标题设置: huanyu
CSS / JS 文件放置地