Poor surface finish
Release Date:
2026-03-20
-
Particles, water stains, oil contamination, fiber contamination, and clouding are present, resulting in uneven gloss, color staining, and a rough surface.
Possible causes:
(1) Machine cleaning materials have not been thoroughly removed;
(2) Raw material contamination/incompatible interference
Proposed solution:
Add HuanYu HY518 anti-fouling agent to eliminate surface tension differences at fouling sites, thereby enhancing the coating’s resistance to contamination. This formulation is suitable for mild soiling or for preventive addition.
Previous page:
2023-11-07
Silver powder is unevenly dispersed.
2026-03-20
2026-03-20
2026-03-20
2026-03-20
2026-03-20
Contact Us
Address: Floor 1, No. 373-1, Xiaoyanjialou, Hongta Village, Yongzheng Subdistrict, Jinzhou District, Dalian City, Liaoning Province
Contact number:+86 198 2433 9728
Fax: 0411-87818331
Email: huanyu_additive@163.com
Copyright © 2026 Dalian Aidesi New Materials Co., Ltd. All rights reserved.
图片alt标题设置: huanyu
CSS / JS 文件放置地